Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers Oxnilon 66-ST-14GF 14% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 66-ST-14GF 14% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
14% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Filler Content 14 %
14 %
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Temperature 23.0 °C
4.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
503 °F
Deflection Temperature at 1.8 MPa (264 psi) 219 °C
426 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 288 - 299 °C
550 - 570 °F
Users viewing this material also viewed the following: