SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm

@Thickness 3.20 mm
0.013 - 0.016 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.010 - 0.013 cm/cm

@Thickness 3.20 mm
0.010 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 53 %
53 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 98.0 MPa
14200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.36 GPa
342 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.02 J/cm
3.78 ft-lb/in
ASTM D256
Dart Drop, Total Energy 40.0 J
29.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 188 °C

@Thickness 3.20 mm
370 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C

@Thickness 3.20 mm
298 °F

@Thickness 0.126 in
unannealed; ASTM D648