| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
| SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
| SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Lexan® IR2840 PC 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit.. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
| SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific .. |
|||
| Melt Flow | 6.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
| Melt Flow | 6.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
Index; ASTM-D1238 |
| Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
| Melt Flow | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
| Melt Flow | 6.0 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.0 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
| SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
| Melt Flow | 6.0 g/10 min @Load 6.60 kg, Temperature 295 °C |
6.0 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D 1238 |
| SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
| Melt Flow | 6.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Techmer ES Plastiblend® ABS 8005 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
| Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/D |
| Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |
|||
| Melt Flow | 6.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
| Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
| Melt Flow | 6.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
| Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
| DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
| Melt Flow | 6.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Diamond Polymers DIAMALOY 1418 Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
| Melt Flow | 6.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
6.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
cm³/10min; ISO 1133 |
| DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
| Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
| Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |
|||
| Melt Flow | 6.0 g/10 min @Load 2.16 kg, Temperature 240 °C |
6.0 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
| Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |
|||