Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ASTM D 638
Flexural Modulus 4.89 GPa
709 ksi
ASTM D 790
Izod Impact, Notched 0.580 J/cm

@Temperature 23.0 °C
1.09 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 179 °C

@Thickness 3.20 mm
354 °F

@Thickness 0.126 in
unannealed; ASTM D 648