Indium Corp. WF-9942 Wave Solder Flux, No-Residue

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. WF-9942 Wave Solder Flux, No-Residue.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
WF-9942 Wave Soldering Flux is a no-clean flux specifically developed for wave soldering, mixed-technology and through-hole electronic assemblies. This formulations provides greater heat stability required for the increases temperatures used in Pb-free wave soldering processes.WF-9942 is formulated to provide a wide process window with excellent solderability, superior hole-fill and reduced solder balling on all surface finishes. this product can be used with Sn/Cu, Sn/Ag/Cu and Sn/Pb alloys.Features:Use with Pb-free and Sn/Pb alloysExcellent solderability on all board finishesSuperior hole-fillReduces solder ballingPhysical Properties Color: ClearJ-STD-004 Flux Type: ORL0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.828 g/cc

@Temperature 25.0 °C
0.828 g/cc

@Temperature 77.0 °F
0.833 g/cc

@Temperature 15.5 °C
0.833 g/cc

@Temperature 59.9 °F
Solids Content 4.37 %
4.37 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Electrical Properties Metric English Comments
Insulation Resistance 6.37e+9 ohm

@Time 605000 sec
6.37e+9 ohm

@Time 168 hour
Control; IPC B24
6.45e+9 ohm

@Time 86400 sec
6.45e+9 ohm

@Time 24.0 hour
Control; IPC B24
8.51e+12 ohm

@Time 86400 sec
8.51e+12 ohm

@Time 24.0 hour
Telcordia GR-78, Control; IPC B25A
8.73e+12 ohm

@Time 346000 sec
8.73e+12 ohm

@Time 96.0 hour
Telcordia GR-78, Control; IPC B25A
Chemical Properties Metric English Comments
Acid Value 36
36