Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding System.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
1.224 g/cc
0.04422 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.0 MPa
7400 psi
Type I, 5 mm/min; ASTM D638
54.0 MPa
7830 psi
5 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa
9280 psi
Type I, 5 mm/min; ASTM D638
66.0 MPa
9570 psi
5 mm/min; ISO 527
Elongation at Break 12 %
12 %
5 mm/min; ISO 527
15 %
15 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.1 %
3.1 %
5 mm/min; ISO 527
5.4 %
5.4 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
2.67 GPa
387 ksi
50 mm/min; ASTM D638
Flexural Strength 101 MPa
14600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 99.0 MPa
14400 psi
2 mm/min; ISO 178
Flexural Modulus 2.56 GPa
371 ksi
2 mm/min; ISO 178
2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.520 J/cm
0.974 ft-lb/in
ASTM D256
Izod Impact, Unnotched 21.6 J/cm
40.5 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 200 kJ/m²
95.2 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
138 °C

@Thickness 3.20 mm
280 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05 - 1.00e+8 ohm-cm
1e+05 - 1.00e+8 ohm-cm
ASTM D257
Surface Resistance 1e+05 - 1.00e+8 ohm
1e+05 - 1.00e+8 ohm
ASTM D257
Static Decay 0.10 sec
0.10 sec
5000V to <50V; FTMS101B
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved