Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® FXE121R PC
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1200-22 Polycarbonate Resin
Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1300-22 Polycarbonate Resin
Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin
Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 3010-22 Polycarbonate Resin
Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201-22 Polycarbonate Resin
Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin
Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 4.00 mm
259 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific)
High heat PPO/HIPS alloy suitable for use in some potable water applications.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Lexan® SFX123RU PC
SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Lexan® SFX123RU PC (Asia Pacific)
SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..
Copyright © lookpolymers.com All Rights Reserved