Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinlab® CYNERGY CA6310 Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Resinlab®
Trade Name CYNERGY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinlab® CYNERGY CA6310 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Application: The CYNERGY SERIES of the cyanoacrylates should be applied in small amounts to one surface only. The parts should then be mated together under slight pressure. This causes the adhesive to spread out into a thin film and assures optimum adhesive performance. The pressure need only be applied for several seconds. The CYNERGY SERIES cures rapidly allowing for bonded parts to be handled within 10 to 60 seconds for most applications. Full cure is normally within 24 hours.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
Adhesive Bond Strength 29.0 MPa
4200 psi
Steel lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time >= 0.208 min
>= 0.00347 hour
Fixture
240 min
4.00 hour
Full cure
Descriptive Properties Value Comments
Base Ethyl
Color Clear
Gap Fill (mil) 10