| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Maxxam™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Maxxam™ FR PP H6 GF25 NHFR grey Polypropylene, Unspecified (PP, Unspecified).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 25.9 MPa | 3760 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 150 % | 150 % | Type I, 51 mm/min; ASTM D638 |
| Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Gardner Impact | 15.8 J @Thickness 3.18 mm, Temperature 23.0 °C |
11.7 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 93.3 °C @Thickness 3.18 mm |
200 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Flammability, UL94 | HB @Thickness 3.18 mm |
HB @Thickness 0.125 in |
NC; UL 94 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | USP Class VI | |
| Features | Flame Retardant | |
| High Impact Resistance | ||
| Low Flow | ||
| Forms | Pellets | |
| Generic Material | PP, Unspecified | |
| Generic Name | Polypropylene, Unspecified (PP, Unspecified) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |