Ravago Manufacturing Americas Enviramid™ N1335STHL BK Post Consumer Recycle Nylon 66, 35% Glass Filled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N1335STHL BK Post Consumer Recycle Nylon 66, 35% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 6.000 GPa
870.2 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648