Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 89.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength at Break 89.6 MPa
13000 psi
2 in/min; ASTM D638
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 89.6 MPa
13000 psi
2 in/min; ASTM D638
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced
Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy
Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
Tensile Strength at Break 89.6 MPa
13000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Albis Plastics PC/PET 748/718 GF 20 HZ 20% Glass Fiber  (discontinued **)
Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled
PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Chase Plastics CP Pryme® N310GL (DAM) Nylon 6 (Utility Grade), 10% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 89.6 MPa
13000 psi
2 in/min; ASTM D638
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved