| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced | 
| Manufacturer | Radici Group Plastics | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Radici Radilon® AHS (dry) Nylon 66.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ISO 1183 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-1/2 | 
| Elongation at Break | 25 % | 25 % | ISO 527-1/2 | 
| Elongation at Yield | 6.5 % | 6.5 % | ISO 524-1/2 | 
| Tensile Modulus | 3.55 GPa | 515 ksi | ISO 527-1/2 | 
| Flexural Strength | 105 MPa | 15200 psi | ISO 178 | 
| Flexural Modulus | 2.95 GPa | 428 ksi | ISO 178 | 
| Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | ISO 179/1eA | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | ISO 1135 7-1-3 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75/2Bf | 
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ISO 75/2Af | 
| Vicat Softening Point | 240 °C | 464 °F | ISO 306 | 
| Flammability, UL94 | V-2 @Thickness 0.800 mm | V-2 @Thickness 0.0315 in |