Material Notes:
Green Fluoroelastomer Rubber, 70-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA). Water and n-Hexane extraction tested in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. ASTM designation = FKM. ISO designation = FPM.Applications: Excellent oil and heat resistance. For repeated use in equipment associated with the production of foodstuffs intended for human consumption. For use with aqueous or fatty foods.
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
°IRHD; ASTM D1415
56 - 86
56 - 86
°IRHD, ±15 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D412
7.00 - 13.0 MPa
1020 - 1890 psi
±30% change after 72 hours @ 250°C; ASTM D412
Elongation at Break 75 %
75 %
-50% change after 72 hours @ 250°C; ASTM D412
150 %
150 %
ASTM D412
Compression Set 13 %
13 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 pass
Distilled Water
pass