Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = 315 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V60B Fluoroelastomer Compound
Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B37, B38, EF31, EO78, F15, Z1. Z1 = compression set..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V60D Fluoroelastomer Compound
Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are re..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V60F Fluoroelastomer Compound
Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V60G Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = colour gr..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V65G Fluoroelastomer Compound
Bright Green Fluoroelastomer Rubber, 60-70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = co..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V70B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V70D Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 70.Applications: Mouldings which are requ..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V70H Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administ..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V70Q Fluoroelastomer Compound
Black, Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. ASTM designation = FKM. ISO designation = FPM. Formulated using only those ingredients determi..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V72H Fluoroelastomer Compound
Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75A Fluoroelastomer Compound
Signal Blue, Fluoroelastomer Rubber, 70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Diesel liner ring grade.Applications: Excellent resistance to oils, fuels and hydraulic flu..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75C Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 70-80 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out:- MHK710, A1-10, B38, EF31, EO78, Z1, Z2,..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75F Fluoroelastomer Compound
Special steam resistant, Fluoroelastomer Rubber, 70-80 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75G Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 70-80 °IRHD. Diesel liner ring grade. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK707, A1-10, B38, EF31, EO78, F..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75L Fluoroelastomer Compound
Special, steam-resistant Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1...
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75M Fluoroelastomer Compound
Brown Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1, Z2. Z1 = comp..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75V Fluoroelastomer Compound
Special steam resistant, Fluoroelastomer Rubber, 70-80 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out MHK707, A1-10, B37, E..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75X Fluoroelastomer Compound
Graphite incorporated, Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V75Y Fluoroelastomer Compound
Yellow Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = co..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V80G Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = gre..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V80Q Fluoroelastomer Compound
Black Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administr..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V85K Fluoroelastomer Compound
Fluoroelastomer Rubber, 80-90 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK910, A1-10, B37, B38, EF31, EO78, Z1. Wher..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V90B Fluoroelastomer Compound
Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M5HK910, A1-11, B38, EF31, EO78, F15, Z1. Where Z1 = compression s..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V90D Fluoroelastomer Compound
Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V90M Fluoroelastomer Compound
Brown Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M3HK914, A1-10, B38, EF31, EO78, Z1, Z2, where Z1 = Brown and..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V90W Fluoroelastomer Compound
Off-White Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admin..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V94E Fluoroelastomer Compound
Special steam resistant, Brown Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M3HK910, A1-10, B38, EF31, EO78, Z1..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V95F Fluoroelastomer Compound
Special steam resistant, Fluoroelastomer Rubber, 85-95 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V97B Fluoroelastomer Compound
Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Wher..
Flash Point >= 315 °C
>= 599 °F
Precision Polymer Engineering V65B Fluoroelastomer Compound
Fluoroelastomer Rubber, 61-70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Copyright © lookpolymers.com All Rights Reserved