Material Notes:
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
75
75
°IRHD, +5 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 12.08 MPa
1752 psi
-20% change after 72 hours @ 250°C; ASTM D412
15.1 MPa
2190 psi
ASTM D412
Elongation at Break 297 %
297 %
-10% change after 72 hours @ 250°C; ASTM D412
330 %
330 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F