Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8103-16 One Part Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8103-16 One Part Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak exotherm 130°C (265°F). At 100°C (212°F), gels in 3-4 hrs, total cure in 4-6 hrs. At 110-120°C (230-250°F) gels to 0.5-1 hr and total cure in 1-2 hrs.
Physical Properties Metric English Comments
Viscosity Measurement 1500
1500
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
Tensile Strength, Ultimate 47.78 MPa
6930 psi
Elongation at Break 14.4 %
14.4 %
Flexural Yield Strength 73.02 MPa
10590 psi
Flexural Modulus 2.12 GPa
307 ksi
Compressive Yield Strength 68.95 MPa
10000 psi
Compressive Modulus 2.21 GPa
321 ksi
Izod Impact, Notched 0.368 J/cm
0.689 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 62.0 °C
144 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 7.52e+14 ohm-cm
7.52e+14 ohm-cm
Surface Resistance 4.71e+14 ohm
4.71e+14 ohm
Dielectric Constant 3.13

@Frequency 1e+6 Hz
3.13

@Frequency 1e+6 Hz
3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
3.46

@Frequency 60 Hz
3.46

@Frequency 60 Hz
Dissipation Factor 0.0044

@Frequency 60 Hz
0.0044

@Frequency 60 Hz
0.012

@Frequency 1000 Hz
0.012

@Frequency 1000 Hz
0.024

@Frequency 1e+6 Hz
0.024

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 360 min

@Temperature 360 °C
360 min

@Temperature 680 °F
500 g
Descriptive Properties Value Comments
Exotherm 130°C
Peak
Users viewing this material also viewed the following: