Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamTal PM3009G5 Acetal, 25% Glass Fiber

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTal PM3009G5 Acetal, 25% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
25% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
DIN 53479
Water Absorption 0.20 %
0.20 %
DIN 53495
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Flexural Strength 150 MPa
21800 psi
ASTM-D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM-D790
Izod Impact, Notched 0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Strength 20.0 kV/mm
508 kV/in
VDE 0303/4
Users viewing this material also viewed the following: