Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
50% mineral filled, heavy density polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
DIN 53479
Linear Mold Shrinkage 0.011 - 0.012 cm/cm
0.011 - 0.012 in/in
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM-D638
Elongation at Break 90 %
90 %
ASTM-D638
Flexural Strength 28.0 MPa
4060 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM-D790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM-D256