SABIC PVC 741E Emulsion Polyvinyl Chloride for Paste Preparation

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PVC 741E Emulsion Polyvinyl Chloride for Paste Preparation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PVC 741E is a fine particle, high molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting low viscosities at low shear rates and slightly dilatant flow characteristics at high shear rates with plasticizer concentrations of 40-60 Phr. Plastisols made from this resin exhibit the following properties:Long shelf life, low viscosity agingLow plastisol viscosityEasy gelationNo tendency toward settling outHigh abrasion resistanceGood thermal stability with a range of standard stabilizersLow percentage of oversized particlesHigh filler toleranceGood drum gellingTypical Applications: Pastes made from PVC 741E are ideal for compact, clear thin coating, and also for chemically blown spread coatings with low plasticizer content. Applications include coatings for conveyor belts, tarpaulins, raincoats, swimming pool liners, tablecloths, wall covering, top coats, handbags, luggage, vinyl-backed carpets, and cushioned vinyl floor coverings.Information provided by SABIC.
Physical Properties Metric English Comments
Bulk Density 0.330 g/cc
0.0119 lb/in³
ISO 60
Volatiles <= 0.30 %
<= 0.30 %
ISO 1269
Particle Size <= 63 µm
<= 63 µm
0.75% retained; ISO 1624
<= 106 µm
<= 106 µm
0.01% retained; ISO 1624
Viscosity 45000 cP

@Pressure 0.621 MPa
45000 cP

@Pressure 90.0 psi
Servers; ASTM D-1823
Brookfield Viscosity 30000 cP
30000 cP
20 rpm; ISO 2555/4575
Descriptive Properties Value Comments
K-Value 74
ISO 1628-2