| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant |
| Manufacturer | Polykemi AB |
| Trade Name | POLYshine |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYshine PBT D203 GF30 FR PBT, Glass Fiber Reinforced, Flame Retardant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
| Filler Content | 30 % | 30 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | With Flow; ISO 2577 |
| 0.012 cm/cm | 0.012 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 145 MPa | <= 21000 psi | ISO/R527 |
| Elongation at Break | 1.8 % | 1.8 % | ISO/R527 |
| Flexural Strength | <= 180 MPa | <= 26100 psi | ISO 178 |
| Flexural Modulus | 8.70 GPa <br>@Temperature 23.0 °C |
1260 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.400 J/cm² <br>@Temperature 23.0 °C |
1.90 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| 0.400 J/cm² <br>@Temperature -20.0 °C |
1.90 ft-lb/in² <br>@Temperature -4.00 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 210 °C <br>@Load 5.001 kg |
410 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | V-0 <br>@Thickness 1.60 mm |
V-0 <br>@Thickness 0.0630 in |
|
| Glow Wire Test | 960 °C <br>@Thickness 2.00 mm |
1760 °F <br>@Thickness 0.0787 in |
IEC 695-2-1 |