| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable Y152 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 17.9 MPa | 2600 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 300 % | 300 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
| Brittleness Temperature | -21.0 °C | -5.80 °F | ASTM D746 |
| Oxygen Index | 24 % <br>@Thickness 1.91 mm |
24 % <br>@Thickness 0.0752 in |
ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 171 - 177 °C | 340 - 351 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | CSA BSS TI1 | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 80% | 121°C, 1.91 mm; 168 hr, UL Standard |
| Retention of Tensile Strength | 100% | 121°C, 1.91 mm; 168 hr, UL Standard |
| Uses | Insulation | |
| Wire & Cable Applications | ||
| Wire Types | THW | |
| TW |