Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
15 sec; ASTM D2240
Tensile Strength, Yield 30.7 MPa
4450 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 180 %
180 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
UL Temperature Rating
Flammability, UL94 V-0

@Thickness 0.749 mm
V-0

@Thickness 0.0295 in
ALL; UL 94
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMFZ2
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Wire & Cable Applications