Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 61 | 61 | 15 sec; ASTM D2240 |
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D638 |
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
Elongation at Break | 360 % | 360 % | 510 mm/min; ASTM D638 |
Tear Strength | 22.8 kN/m | 130 pli | Die C, 510 mm/min; ASTM D624 |
Compression Set | 30 % @Temperature 23.0 °C, Time 79200 sec |
30 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -36.7 °C | -34.1 °F | ASTM D746 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 168 - 174 °C | 334 - 345 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Features | General Purpose | |
Low Gloss | ||
Forms | Pellets | |
Generic Material | PVC, Flexible | |
Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
Processing Method | Extrusion | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
Uses | General Purpose |