Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 2542 Non-Conductive Extruded Elastomer Specifications Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL or CHO-SIL conductive elastomers are extruded in parallel with non-conductiv.. |
|||
Tensile Strength | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tensile Strength | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® 862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tensile Strength | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tensile Strength | 3.45 MPa | 500 psi | ASTM D412 |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 0860 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.45 MPa @Strain 100 % |
500 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.45 MPa | 500 psi | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 3.45 MPa | 500 psi | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 3.45 MPa | 500 psi | |
Lucite International Elvacite ® 2044 Acrylic Resin Elvacite® 2044 is a high molecular weight n-butyl methacrylate polymer. Elvacite® 2044 is useful in adhesives for smooth plastic films and aluminum, and in silk screen inks. It will plasticize.. |
|||
Tensile Strength | 3.45 MPa | 500 psi | |
Teknor Apex Tekbond® TB 1413A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |