| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | PolyOne Corporation |
| Trade Name | Edgetek® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Edgetek® PE-30GF/000 Polyethylene, High Density (HDPE).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 41.4 MPa | 6000 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 4.14 GPa | 600 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 116 °C @Thickness 3.18 mm |
241 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 193 - 221 °C | 379 - 430 °F | |
| Mold Temperature | 26.7 - 54.4 °C | 80.1 - 130 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Filler / Reinforcement | Glass Fiber Reinforcement | |
| Forms | Pellets | |
| Generic Material | HDPE | |
| Generic Name | Polyethylene, High Density (HDPE) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |