DuPont Elvax® 150 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 150 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compounding and extrusion; and wire and cable.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792-ISO 1183, ASTM D1505
Vinyl Acetate Content 32 %
32 %
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
ASTM D2240-ISO 868
Hardness, Shore D 24
24
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Melting Point 63.0 °C
145 °F
ASTM D3417
Vicat Softening Point 36.0 °C
96.8 °F
ASTM D1525, ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D746
Ring & Ball Softening Point 110 °C
230 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 102
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.