Zeon Chemicals Nipol® NX775 Carboxylated Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® NX775 Carboxylated Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nipol NX775 is a cold polymerized, butadiene-acrylonitrile-carboxylic acid terpolymer. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent processing with conventional coated zinc oxides. High performance injection molding, rolls, calendered belting and extruded hose. Fast cure rate. Carboxyl content is 0.083 EPHR.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Mooney Viscosity 38 - 52

@Temperature 100 °C
38 - 52

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 1.0 %
<= 1.0 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 23.6-28.7
Carboxyl Content, % 0.067-0.099
Heat Loss (%) Max 0.6
Hot/Cold C
Mooney Scorch MS, Min 5