Zeon Chemicals Hydrin® H-45 Epichlorohydrin Homopolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Hydrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Hydrin® H-45 Epichlorohydrin Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrin H-45 is an epichlorohydrin homopolymer with high oil, fuel and solvent resistance. Compounds using Hydrin H-45 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.An epichlorohydrin homopolymer with high oil, fuel and solvent resistance. Has good heat resistance, excellent ozone resistance along with outstanding gas impermeability.
Physical Properties Metric English Comments
Mooney Viscosity 40 - 50

@Temperature 100 °C
40 - 50

@Temperature 212 °F
(1+4); ASTM D1646
Ash <= 0.50 %
<= 0.50 %
Zeon Test #1358
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361