Plansee MT11 Molybdenum-Tantalum

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer Plansee SE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee MT11 Molybdenum-Tantalum.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Outstanding corrosion resistance properties, highly suitable for touch-screen applicationsInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 10.9 g/cc
10.9 g/cc
Calculated
Component Elements Properties Metric English Comments
Molybdenum, Mo 89 %
89 %
Balance
Tantalum, Ta 11 %
11 %