Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.930 - 1.04 g/cc
0.0336 - 0.0376 lb/in³
Average value: 0.957 g/cc Grade Count:16
Methyl Acrylate Content 10.0 - 24.0 %
10.0 - 24.0 %
Average value: 19.1 % Grade Count:6
Melt Flow 1.00 - 60.0 g/10 min
1.00 - 60.0 g/10 min
Average value: 16.8 g/10 min Grade Count:15
Mechanical Properties Metric English Comments
Hardness, Shore A 79.0 - 86.0
79.0 - 86.0
Average value: 82.7 Grade Count:3
Hardness, Shore D 26.0 - 48.0
26.0 - 48.0
Average value: 35.0 Grade Count:7
Tensile Strength, Ultimate 8.00 - 13.0 MPa
1160 - 1890 psi
Average value: 10.2 MPa Grade Count:7
Elongation at Break 475 - 925 %
475 - 925 %
Average value: 764 % Grade Count:7
Flexural Modulus 0.0190 - 0.0372 GPa
2.76 - 5.40 ksi
Average value: 0.0274 GPa Grade Count:3
Dart Drop, Total Energy 32.5397 - 32.5397 J

@Temperature -40.0 - -40.0 °C
24.0000 - 24.0000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 32.5 J Grade Count:1
Thermal Properties Metric English Comments
Melting Point 64.0 - 95.0 °C
147 - 203 °F
Average value: 78.8 °C Grade Count:8
Vicat Softening Point 39.0 - 71.0 °C
102 - 160 °F
Average value: 52.1 °C Grade Count:7
Brittleness Temperature -73.0 - -60.0 °C
-99.4 - -76.0 °F
Average value: -69.8 °C Grade Count:4