| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
| Elongation at Break | 40 % | 40 % | ISO 527 |
| Flexural Strength | 160 MPa | 23200 psi | ISO 178 |
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/A |
| Izod Impact, Unnotched (ISO) | NB | NB | ISO 180/U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
| Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO75A |
| Flammability, UL94 | V-0 <br>@Thickness 0.400 mm |
V-0 <br>@Thickness 0.0157 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ISO 60093 |
| Dielectric Constant | 3.2 <br>@Frequency 1000 Hz |
3.2 <br>@Frequency 1000 Hz |
ISO 60250 |
| Dissipation Factor | 0.0033 <br>@Frequency 1000 Hz |
0.0033 <br>@Frequency 1000 Hz |
ISO 60250 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets |