| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled | 
| Manufacturer | Polymer Technology & Services, LLC (PTS) | 
| Trade Name | Trimid® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | PTS Trimid® N6-TG30L-BK 30% Glass Fiber, High Impact Nylon 6.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 | 
| Elongation at Break | 4.5 % | 4.5 % | ASTM D638 | 
| Flexural Modulus |           8.00           GPa           @Thickness 3.17 mm  | 
                  1160           ksi           @Thickness 0.125 in  | 
        ASTM D790 | 
| Izod Impact, Notched |           1.98           J/cm           @Thickness 3.17 mm  | 
                  3.71           ft-lb/in           @Thickness 0.125 in  | 
        ASTM D256 | 
| Izod Impact, Unnotched |           5.34           J/cm           @Thickness 3.17 mm  | 
                  10.0           ft-lb/in           @Thickness 0.125 in  | 
        
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | >= 200 °C | >= 392 °F | ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ASTM D648 | 
| Flammability, UL94 |           HB                     @Thickness 1.57 mm  | 
                  HB                     @Thickness 0.0620 in  |