Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Daikin NEOFLON AP-211SH PFA Semiconductor Grade

Category Polymer , Thermoplastic , Fluoropolymer , PFA , Polyperfluoroalkoxyethylene, Molded/Extruded
Manufacturer Daikin Industries
Trade Name NEOFLON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Daikin NEOFLON AP-211SH PFA Semiconductor Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NEOFLON PFA semiconductor grade.Applications: Tubing and injection molded parts requiring high stress crack resistance, etc.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
at 25°C
Bulk Density 1.20 g/cc
0.0434 lb/in³
Melt Flow 10 - 18 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 18 g/10 min

@Load 11.0 lb,
Temperature 702 °F
Mechanical Properties Metric English Comments
Coefficient of Friction 0.040 - 0.060
0.040 - 0.060
Taber Abrasion, mg/1000 Cycles <= 96.75
<= 96.75
9.8 N load, cs-10 wheel
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
Electrical Properties Metric English Comments
Dielectric Constant 1.92 - 2.12

@Frequency 1000 Hz
1.92 - 2.12

@Frequency 1000 Hz
ASTM D150
1.92 - 2.12

@Frequency 1e+6 Hz
1.92 - 2.12

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00010 - 0.00021
0.00010 - 0.00021