Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 - 106 °C | 176 - 223 °F | Average value: 94.3 °C Grade Count:52 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 42.0 - 106 °C | 108 - 223 °F | Average value: 72.4 °C Grade Count:25 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.8 - 106 °C | 190 - 223 °F | Average value: 94.4 °C Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 - 106 °C | 196 - 223 °F | Average value: 100 °C Grade Count:7 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |