Nanocyl PLASTICYL™ PA1502 Polyamide 12 with Multi-Wall Carbon Nanotubes

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Carbon Fiber Filled
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ PA1502 Polyamide 12 with Multi-Wall Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PA1502 is a conductive masterbatch based on polyamide 12. Because of its high flow formulation, PLASTICYL™ PA1502 is ideal for standard injection molding and extrusion processes.Applications:ESD (Electrostatic Discharge) and electrically conductive partsE&E, automotive, industrialInjection molding, extrusionBenefits:Electrical conductivity at low loadingRetention of key mechanical propertiesEasier processing
Physical Properties Metric English Comments
Specific Gravity 1.081 g/cc
1.081 g/cc
ISO 1183
Filler Content 14 - 16 %
14 - 16 %
Carbon Nanotube Loading
High Load Melt Index <= 3.14 g/10 min

@Load 15.0 kg,
Temperature 300 °C
<= 3.14 g/10 min

@Load 33.1 lb,
Temperature 572 °F
4 mm; Non-standard Test
Thermal Properties Metric English Comments
Melting Point 179 °C
354 °F
Masterbatch; ISO 11357-1,-3