Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength, Yield 22.1 MPa
3200 psi
at max load; ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Gardner Impact >= 40.7 J
>= 30.0 ft-lb
>= 40.7 J

@Temperature -28.9 °C
>= 30.0 ft-lb

@Temperature -20.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648