| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
NYCOA 1417 HS Heat Stabilized, Impact Modified Nylon 6 Resin
NYCOA 1417 HS is a heat stabilized and impact modified Nylon 6. This medium viscosity resin was developed for injection molding and extrusion processes for applications requiring improved toughness,..
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
NYCOA 2011 Copolymer Nylon
impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
NYCOA 27/440KNF Glass Filled Nylon 6
44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc.
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer
Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici..
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific)
Multi purpose V1 grade
|
|||
| Izod Impact, Notched |
1.75
J/cm <br>@Temperature -30.0 °C
|
3.28
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics NORYL PX0844 PPE+PS
PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned
Ultra high-rigidityInformation provided by Unitika Ltd.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM-D256 |
|
Braskem AC59 HDPE Monofilament Polyethylene Homopolymer
AC59 resin is a high-density polyethylene homopolymer produced by the solution process and designed for monofilament applications. It contains antioxidant additives. Its applications include: film ..
|
|||
| Izod Impact, Notched | 1.75 J/cm | 3.28 ft-lb/in | ASTM-D256 |
|
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer
GF4950HS resin is a high-density polyethylene (HDPE), bimodal copolymer offering a combination of good processability and environmental stress crack resistance (ESCR). It is thus recommended for the..
|
|||