Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® TE-0546-GBK Hexene MDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF NOVA Chemicals Novapol® TE-0546-GBK Hexene MDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Very good impact, Excellent ESCR, Sub 50 mesh particles sizeApplications: Powder coating of pipes, values, and fittings to produce a corrosion-resistant coating for buried pipe systemsAdditives: Antioxidants and processing stabilizers, UV stabilizers, Carbon blackInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Base Resin; ASTM D792
0.946 g/cc
0.0342 lb/in³
Compounded; ASTM D792
Water Absorption 0.010 %
0.010 %
ASTM D570
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F<sub>50</sub>; Condition B, 100% Igepal; ASTM D1693
Oxidative Induction Time (OIT) 10 min
10 min
Condition 220°C, in oxygen environment; ASTM D3895
Melt Flow 5.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
Extension rate 2 in/min; ASTM D638
Elongation at Break 800 %
800 %
Extension rate 2 in/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
ASTM D3417
Vicat Softening Point 111 °C
232 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Descriptive Properties Value Comments
Filler % 2.5
Carbon Black per ASTM D4218
Users viewing this material also viewed the following: