Multibase Multi-Flex® TPE A 8620 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8620 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Formulated TPE compound is based on Shell's Kraton G resin and is widely used in automotive applications exhibiting a wide temperature range, replacing in many applications conventional thermoset rubber. Multibase is a licensed compounder for Shell's Kraton G polymers. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
10 sec; ASTM D-2240
Tensile Strength, Ultimate 10.3 MPa
1490 psi
ASTM D412
Elongation at Break 925 %
925 %
ASTM D412
Flexural Modulus 0.137 GPa
19.9 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 54.3 kN/m
310 pli
ASTM D624