Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ASTM 792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
10 seconds; ASTM D2240
Tensile Strength, Yield 20.7 MPa
3000 psi
Elastic; ASTM D412
Elongation at Break 150 %
150 %
Elastic; ASTM D412
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Tear Strength 78.9 kN/m
450 pli
ASTM D624
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Front Barrel Temperature 221 - 232 °C
430 - 450 °F
Nozzle Temperature 6.11 - 232 °C
43.0 - 450 °F
Melt Temperature 232 °C
450 °F
Mold Temperature 37.8 °C
100 °F
Descriptive Properties Value Comments
Clamp Tonnage 2-4 tons/in<sup>2</sup>
Screw L/D Ratio 20:1