| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792-91 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955-89 |
| Melt Flow | 5.0 g/10 min | 5.0 g/10 min | (Condition G) ASTM D-1238-94a |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 98 | 98 | ASTM D785-95 |
| Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | ASTM D638-95 |
| Elongation at Break | 50 % | 50 % | ASTM D638-95 |
| Flexural Modulus | 2.276 GPa | 330.1 ksi | RT; ASTM D-790-95 |
| Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256-93a |
| Gardner Impact | 31.1 J | 22.9 ft-lb | ASTM D5420-93 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 175 °C | 347 °F | injection molded unannealed; ASTM D-648-95 |
| 220 °C | 428 °F | injection molded annealed; ASTM D-648-95 | |
| 220 °C | 428 °F | compression molded annealed; ASTM D-648-95 | |
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525-95 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
|
| HB @Thickness 3.17 mm |
HB @Thickness 0.125 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 85 - 90 % | 85 - 90 % | ASTM D2457-90 |