Polymer Property : Maximum Service Temperature, Air = 399 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease
CHO-LUBE 4220 conductive grease is based on silicone fluid, which is characterized by unusual chemical inertness and outstanding thermal stability. It is a silver-filled lubricant designed for surfa..
Maximum Service Temperature, Air 204 °C
399 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Contractors SCS 1000® Construction Sealant
One-part, for general purpose glazing and sealing applications. Cure Method: Acetoxy. Tack-free time
Maximum Service Temperature, Air 204 °C
399 °F
Continuous
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Momentive Performance Materials RTV21 Pink General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Maximum Service Temperature, Air 204 °C
399 °F
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
Maximum Service Temperature, Air 204 °C
399 °F
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 100 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor..
Maximum Service Temperature, Air 204 °C
399 °F
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea..
Maximum Service Temperature, Air 204 °C
399 °F
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal..
Maximum Service Temperature, Air 204 °C
399 °F
Dow Corning 111 VALVE LUBRICANT & SEALANT
General purpose O-ring and valve lubricant. Provides a noncuring moisture barrier; high dielectric strength; moisture and ozone resistance; good thermal, oxidation and chemical stability; suitable ..
Maximum Service Temperature, Air 204 °C
399 °F
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo..
Maximum Service Temperature, Air 204 °C
399 °F
continuous
Arlon Red Silicone Press Pad with Fiberglass Substrate (55393R045)
Side one - cured silicone rubber, 0.014 in. (0.36 mm) minimum; Substrate - Prime Coated 162 Fiberglass, 0.018 in. (0.46 mm) nominal; Side two - cured silicone rubber, 0.013 in. (0.33 mm) minimum; 0...
Maximum Service Temperature, Air 204 °C
399 °F
continuous
Arlon Red Silicone Press Pad with sandwiched Fiberglass Substrate (55393R062)
Cured silicone rubber with a minimum thickness of 0.027 in. (0.69 mm)/0.018 in. (0.46 mm) Prime Coated 162 Fiberglass/Cured silicone rubber with a minimum thickness of 0.017 in. (0.43 mm); 0.003 in...
Maximum Service Temperature, Air 204 °C
399 °F
cured 10 mins @ 150°C
ACC QLE 1050 QSI Quantum Silicones 30 Durometer Clear, Addition Cure, 1-part Elastomer for Coating
QLE 1050 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: 100% solids Transparent, ideal for pigmentat..
Maximum Service Temperature, Air 204 °C
399 °F
ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material
QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..
Maximum Service Temperature, Air 204 °C
399 °F
3M 8902 Polyester Tape
3M™ Polyester Tape 8902 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi..
Maximum Service Temperature, Air 204 °C
399 °F
3M Scotch-Weld™ GM10 Gasket Maker Anaerobic Adhesive
3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal..
Maximum Service Temperature, Air 204 °C
399 °F
Henkel Hysol EA 9396/C-2 Paste Adhesive System
Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding