Polymer Property : Density = 0.0337 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D 792
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin
IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Density 0.932 g/cc
0.0337 lb/in³
ASTM D792
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D4883
Eastman M3006-P Polyethylene  (discontinued **)
Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properti..
Density 0.932 g/cc
0.0337 lb/in³
ASTM D4883
Eastman M3019-P Polyethylene  (discontinued **)
M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D1505
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer
The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D1505
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibi..
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 115-1327 LMDPE Rotational Molding Resin
Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene..
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 324-1327 LMDPE Rotational Molding Resin
Description: ICORENE 324-1327 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D1505-98
Ipiranga Petrochem MB 0434 LS-L MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Density 0.933 g/cc
0.0337 lb/in³
ISO 1183
Iran Petrochemical (PCC) MF3313 High Density Polyethylene
MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co.
Density 0.932 g/cc
0.0337 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/2 Polyolefin
Catalyst CT/2 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it all..
Density 0.932 g/cc
0.0337 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/2-LR Polyolefin
Catalyst CT/2-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it ..
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding
Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons..
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding
Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding
Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons..
Density 0.932 g/cc
0.0337 lb/in³
ISO 1183
Borealis Himod™ FT7324 . LDPE for Film
Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Density 0.933 g/cc
0.0337 lb/in³
LE 4437; ASTM D792
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation
Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of..
Density 0.933 g/cc
0.0337 lb/in³
Catalyst LE 4476; ASTM D792
Borealis Visico™/Ambicat™ ME4425/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation
Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4476, will undergo an accelerated, moisture-induced crosslinking reaction. Th..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D792-ISO 1183
DuPont Elvax® 670 Ethylene Vinyl Acetate
DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding ..
Density 0.934 g/cc
0.0337 lb/in³
Result
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications
Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D1505
Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE.Applic..
Density 0.933 g/cc
0.0337 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin
Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl..
Density 0.932 g/cc
0.0337 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Density 0.933 g/cc
0.0337 lb/in³
ASTM D792
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Density 0.932 g/cc
0.0337 lb/in³
ISO 1183
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound
Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds..
Density 0.932 g/cc
0.0337 lb/in³
Melt; ISO 1183
BASF Ultramid® 8202 HS PA6 (Conditioned)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Density 0.932 - 1.64 g/cc
0.0337 - 0.0592 lb/in³
Average value: 1.19 g/cc Grade Count:114
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Density 0.933 g/cc
0.0337 lb/in³
compound; ISO 1183
Borealis LE6025 Polyethylene Modified Jacketing Compound
LE6025 is a black low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in combinat..