Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360)

Category Metal , Nonferrous Metal , Beryllium Alloy , Nickel Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name Nibryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.28 g/cc
0.299 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1035 MPa
>= 150100 psi
Tensile Strength, Yield >= 690 MPa
>= 100000 psi
Elongation at Break >= 20 %
>= 20 %
Modulus of Elasticity 207 GPa
30000 ksi
Thermal Properties Metric English Comments
CTE, linear 14.0 µm/m-°C

@Temperature 20.0 - 200 °C
7.78 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Melting Point 1196 - 1330 °C
2185 - 2430 °F
Solidus 1196 °C
2185 °F
Liquidus 1330 °C
2430 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.85 - 2.05 %
1.85 - 2.05 %
Nickel, Ni 97.5 %
97.5 %
as balance
Titanium, Ti 0.40 - 0.60 %
0.40 - 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm
(7% IACS Conductivity)