Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of meeting UL 1581 VW-1 requirement. 90C or 105C temperature rating as defined by UL 62 TPE category. 85 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 250 °C
16 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
30S reading; ASTM D2240
Tensile Strength at Break 16.0 MPa
2320 psi
50 mm/min; ISO 527
16.0 MPa
2320 psi
Type I, 50 mm/min; ASTM D638
22.0 MPa
3190 psi
after 7days @136°C; UL 1581
23.0 MPa
3340 psi
UL 1581
Elongation at Break 250 %
250 %
50 mm/min; ISO 527
251 %
251 %
after 7days @136°C; UL 1581
260 %
260 %
Type I, 50 mm/min; ASTM D638
308 %
308 %
UL 1581
Flexural Modulus 0.0400 GPa
5.80 ksi
12.5 mm/min; ISO 178
0.0600 GPa
8.70 ksi
12.5 mm/min, 100 mm span; ASTM D790
Heat Distortion 5.0 %

@Load 0.250 kg,
Temperature 121 °C
5.0 %

@Load 0.551 lb,
Temperature 250 °F
UL 1581
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 26 %
26 %
ISO 4589
Glow Wire Test 825 °C
1520 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+16 ohm-cm
1.90e+16 ohm-cm
ASTM D257
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0070

@Frequency 1.00e+6 Hz
0.0070

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 110
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 47
ASTM E 662
VW-1 Pass
UL 1581