SABIC HP7022 Low Density Polyethylene for Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC HP7022 Low Density Polyethylene for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: HP7022 is a Low Density Polyethylene offering a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7022 exhibit excellent impact strength, low shrinkage and good gloss.Typical Applications: HP7022 is intended for producing flexible injection molded articles. It is particularly suited for closures, caps, lids, housewares articles, toys and as base resin for masterbatch.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 7.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 88 %
88 %
ASTM D638
1% Secant Modulus >= 170 MPa
>= 24700 psi
ASTM D638
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 75 %
75 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F