Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® M4621 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® M4621 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste disposal drums, and specialty injection molded parts.Regulatory StatusM 4621 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing M 4621 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 2.2 g/10 min
2.2 g/10 min
ASTM D1238
Spiral Flow 23.4 cm
9.20 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 14.3 MPa
2080 psi
ASTM D638
Tensile Strength, Yield 24.5 MPa
3560 psi
Crosshead speed - 2"min.; ASTM D638
Elongation at Yield 9.0 %
9.0 %
Crosshead speed - 2"min.; ASTM D638
1% Secant Modulus 1010 MPa
146000 psi
Crosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 0.834 GPa
121 ksi
Crosshead speed - 0.5" min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746