Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® ETP H4837 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon® ETP
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Alathon® ETP H4837 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsALATHON H 4837 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as 4, 5, and 6-quart ice cream containers, which are produced at high speeds in fast cycling multi-cavity stack molds.Regulatory StatusH 4837 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Processing TechniquesSpecific recommendations for processing H 4837 can only be made when the processing conditions, equipment and end use application are known. However, melt temperatures from 475°F to 535°F are recommended for initial start-ups. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 40 g/10 min
40 g/10 min
ASTM D1238
Spiral Flow 46.7 cm
18.4 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength at Break 22.1 MPa
3200 psi
ASTM D638
Tensile Strength, Yield 25.0 MPa
3630 psi
Crosshead speed - 2"min.; ASTM D638
Elongation at Yield 7.9 %
7.9 %
Crosshead speed - 2" min; ASTM D638
1% Secant Modulus 979 MPa
142000 psi
Crosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 0.862 GPa
125 ksi
Crosshead speed - 0.5" min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °C
147 °F
ASTM D648
Vicat Softening Point 121 °C
250 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746