Techmer ES Statiblend® POM CO

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® POM CO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 3.5 g/10 min

@Load 10.0 kg,
Temperature 230 °C
3.5 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+8 ohm-cm
1.00e+6 - 1.00e+8 ohm-cm
ASTM D257
Surface Resistance 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257