Lucite International Diakon® TD525 Toughened Acrylic Compound

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Lucite International
Trade Name Diakon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Diakon® TD525 Toughened Acrylic Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 1.9 g/10 min
1.9 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 60
60
ISO 2039-2
Tensile Strength 58.0 MPa
8410 psi
ISO 527
Elongation at Break 20 %
20 %
ISO 527
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 3.20 kJ/m²
1.52 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
3.80 J/cm²
18.1 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 103 µm/m-°C
57.2 µin/in-°F
ASTM E831
Vicat Softening Point 101 °C
214 °F
ISO 306B
111 °C
232 °F
ISO 306A
Heat Distortion Temperature 92.0 °C
198 °F
ISO 75A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003